WEKO3
インデックスリンク
アイテム
{"_buckets": {"deposit": "6e53c97a-b2b3-4870-927f-66a4f273e0b5"}, "_deposit": {"created_by": 3, "id": "29331", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "29331"}, "status": "published"}, "_oai": {"id": "oai:kanazawa-u.repo.nii.ac.jp:00029331", "sets": ["1981"]}, "author_link": ["50406", "15733", "50407", "16005"], "item_4_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2008-12-28", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "4", "bibliographicPageEnd": "260", "bibliographicPageStart": "255", "bibliographicVolumeNumber": "47", "bibliographic_titles": [{"bibliographic_title": "粘土科学 = Journal of the Clay Science Society of Japan"}]}]}, "item_4_description_21": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Adsorption and post-adsorption characteristics of different oxyanions such as P, Cr, As and Se onto schwertmannite were investigated in order to understand the role of schwertmannite in acid mine drainage, and its performance and safety assessment in remediation system. Synthetic schwertmannite was used for the adsorption and post-adsorption experiments as a starting material. In the adsorption experiments, the starting material was reacted with various oxyanion solutions such as Na_2HPO_4, Na_2CrO_4・4H_2O, Na_2HAsO_4・7H_2O and Na_2SeO_4 with concentration up to 2.0mM at around pH 3.9. Dominant chemical species of the oxyanions in the experimental condition were thermodynamically calculated as H_2PO_4^-, HCrO_4^-, H_2AsO_4^- and SeO_4^\u003c2-\u003e by Geochemist\u0027s Workbench. The obtained adsorption isotherms showed that the schwertmannite has selectivity for oxyanions during adsorption with the affinity sequence being H_2AsO_4^-\u003eH_2PO_4^-\u003eHCrO_4^-\u003eSeO_4^\u003c2-\u003e. This sequence corresponds to the sequence of decreasing ionic potential of the anions, which suggest that the observed selectivity of schwertmannite could not be attributed to the electrostatic interaction between the oxyanions and schwertmannite. It is known that oxyanions with low ionic potential have a tendency to form inner-sphere complexation with mineral surfaces. Therefore, the observed order of oxyanion retention may correspond to the sequence in affinity for the inner-sphere complexation on schwertmannite. This is also supported by the results of zeta potential measurement, which showed greater decrease of zeta potential after H_2AsO_4^- and H_2PO_4^- adsorption compared to other onyanions. In post-adsorption experiments (aging experiments), transformation to goethite was observed in X-ray diffraction patterns for the schwertmannite containing oxyanions with lower selectivity such as SeO-4^\u003c2-\u003e and SO_4^\u003c2-\u003e while there is no change in X-ray diffraction patterns of schwertmannite with H_2AsO_4^- and H_2PO_4^- even after 556 hours. Desorption of SeO_4^\u003c2-\u003e and SO_4^\u003c2-\u003e was observed prior to the transformation, although most of H_2AsO_4^- and H_2PO_4^- were retained onto schwertmannite. The desorption of oxyanions therefore resulted in the transformation of schwertmannite to goethite. Oxyanions with higher adsorption affinity, i.e., lower ionic potential, have a greater stabilizing effect on schwertmannite structure, although ordinary schwertmannite with SO_4^\u003c2-\u003e is metastable and easily transforms to goethite.", "subitem_description_type": "Abstract"}]}, "item_4_description_5": {"attribute_name": "提供者所属", "attribute_value_mlt": [{"subitem_description": "金沢大学環日本海域環境研究センター", "subitem_description_type": "Other"}]}, "item_4_publisher_17": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本粘土学会 = the Clay Science Society of Japan"}]}, "item_4_relation_28": {"attribute_name": "関連URI", "attribute_value_mlt": [{"subitem_relation_type_id": {"subitem_relation_type_id_text": "http://www.cssj2.org/", "subitem_relation_type_select": "URI"}}, {"subitem_relation_type_id": {"subitem_relation_type_id_text": "https://www.jstage.jst.go.jp/browse/jcssjnendokagaku1961/-char/ja/", "subitem_relation_type_select": "URI"}}, {"subitem_relation_type_id": {"subitem_relation_type_id_text": "http://ci.nii.ac.jp/naid/110007046037/", "subitem_relation_type_select": "URI"}}]}, "item_4_rights_23": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "Copyright © 日本粘土学会 Clay Science Society of Japan | 許可を得て登録"}]}, "item_4_source_id_11": {"attribute_name": "NCID", "attribute_value_mlt": [{"subitem_source_identifier": "AA1155672X", "subitem_source_identifier_type": "NCID"}]}, "item_4_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0470-6455", "subitem_source_identifier_type": "ISSN"}]}, "item_4_version_type_25": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "高田, 盛生"}], "nameIdentifiers": [{"nameIdentifier": "50406", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "福士, 圭介"}], "nameIdentifiers": [{"nameIdentifier": "16005", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "90444207", "nameIdentifierScheme": "金沢大学研究者情報", "nameIdentifierURI": "http://ridb.kanazawa-u.ac.jp/public/detail.php?kaken=90444207"}, {"nameIdentifier": "90444207", "nameIdentifierScheme": "研究者番号", "nameIdentifierURI": "https://nrid.nii.ac.jp/nrid/1000090444207"}]}, {"creatorNames": [{"creatorName": "佐藤, 努"}], "nameIdentifiers": [{"nameIdentifier": "15733", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "10313636", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=10313636"}, {"nameIdentifier": "10313636", "nameIdentifierScheme": "研究者番号", "nameIdentifierURI": "https://nrid.nii.ac.jp/nrid/1000010313636"}]}, {"creatorNames": [{"creatorName": "米田, 哲郎"}], "nameIdentifiers": [{"nameIdentifier": "50407", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2017-10-05"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "SC-PR-FUKUSHI-K-255.pdf", "filesize": [{"value": "688.4 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 688400.0, "url": {"label": "SC-PR-FUKUSHI-K-255.pdf", "url": "https://kanazawa-u.repo.nii.ac.jp/record/29331/files/SC-PR-FUKUSHI-K-255.pdf"}, "version_id": "7f0faea9-6744-4a93-877f-092b21bc505c"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Adsorption", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Schwertmannite", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Surface complexation", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Transformation", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "シュベルトマナイトへの様々なオキシ陰イオンの吸着とその後の安定性", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "シュベルトマナイトへの様々なオキシ陰イオンの吸着とその後の安定性"}, {"subitem_title": "Adsorption of Oxyanions and Post-Adsorption Behavior of Schwertmannite", "subitem_title_language": "en"}]}, "item_type_id": "4", "owner": "3", "path": ["1981"], "permalink_uri": "http://hdl.handle.net/2297/35947", "pubdate": {"attribute_name": "公開日", "attribute_value": "2017-10-05"}, "publish_date": "2017-10-05", "publish_status": "0", "recid": "29331", "relation": {}, "relation_version_is_last": true, "title": ["シュベルトマナイトへの様々なオキシ陰イオンの吸着とその後の安定性"], "weko_shared_id": -1}
シュベルトマナイトへの様々なオキシ陰イオンの吸着とその後の安定性
http://hdl.handle.net/2297/35947
http://hdl.handle.net/2297/35947c788e5a5-0a71-4550-bdfb-87946ac593d8
名前 / ファイル | ライセンス | アクション |
---|---|---|
SC-PR-FUKUSHI-K-255.pdf (688.4 kB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2017-10-05 | |||||
タイトル | ||||||
タイトル | シュベルトマナイトへの様々なオキシ陰イオンの吸着とその後の安定性 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | Adsorption of Oxyanions and Post-Adsorption Behavior of Schwertmannite | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
著者 |
高田, 盛生
× 高田, 盛生× 福士, 圭介× 佐藤, 努× 米田, 哲郎 |
|||||
提供者所属 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 金沢大学環日本海域環境研究センター | |||||
書誌情報 |
粘土科学 = Journal of the Clay Science Society of Japan 巻 47, 号 4, p. 255-260, 発行日 2008-12-28 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0470-6455 | |||||
NCID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AA1155672X | |||||
出版者 | ||||||
出版者 | 日本粘土学会 = the Clay Science Society of Japan | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Adsorption and post-adsorption characteristics of different oxyanions such as P, Cr, As and Se onto schwertmannite were investigated in order to understand the role of schwertmannite in acid mine drainage, and its performance and safety assessment in remediation system. Synthetic schwertmannite was used for the adsorption and post-adsorption experiments as a starting material. In the adsorption experiments, the starting material was reacted with various oxyanion solutions such as Na_2HPO_4, Na_2CrO_4・4H_2O, Na_2HAsO_4・7H_2O and Na_2SeO_4 with concentration up to 2.0mM at around pH 3.9. Dominant chemical species of the oxyanions in the experimental condition were thermodynamically calculated as H_2PO_4^-, HCrO_4^-, H_2AsO_4^- and SeO_4^<2-> by Geochemist's Workbench. The obtained adsorption isotherms showed that the schwertmannite has selectivity for oxyanions during adsorption with the affinity sequence being H_2AsO_4^->H_2PO_4^->HCrO_4^->SeO_4^<2->. This sequence corresponds to the sequence of decreasing ionic potential of the anions, which suggest that the observed selectivity of schwertmannite could not be attributed to the electrostatic interaction between the oxyanions and schwertmannite. It is known that oxyanions with low ionic potential have a tendency to form inner-sphere complexation with mineral surfaces. Therefore, the observed order of oxyanion retention may correspond to the sequence in affinity for the inner-sphere complexation on schwertmannite. This is also supported by the results of zeta potential measurement, which showed greater decrease of zeta potential after H_2AsO_4^- and H_2PO_4^- adsorption compared to other onyanions. In post-adsorption experiments (aging experiments), transformation to goethite was observed in X-ray diffraction patterns for the schwertmannite containing oxyanions with lower selectivity such as SeO-4^<2-> and SO_4^<2-> while there is no change in X-ray diffraction patterns of schwertmannite with H_2AsO_4^- and H_2PO_4^- even after 556 hours. Desorption of SeO_4^<2-> and SO_4^<2-> was observed prior to the transformation, although most of H_2AsO_4^- and H_2PO_4^- were retained onto schwertmannite. The desorption of oxyanions therefore resulted in the transformation of schwertmannite to goethite. Oxyanions with higher adsorption affinity, i.e., lower ionic potential, have a greater stabilizing effect on schwertmannite structure, although ordinary schwertmannite with SO_4^<2-> is metastable and easily transforms to goethite. | |||||
権利 | ||||||
権利情報 | Copyright © 日本粘土学会 Clay Science Society of Japan | 許可を得て登録 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | http://www.cssj2.org/ | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://www.jstage.jst.go.jp/browse/jcssjnendokagaku1961/-char/ja/ | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | http://ci.nii.ac.jp/naid/110007046037/ |