{"_buckets": {"deposit": "dbc815ca-50d2-4160-9822-c65fe0b3bce2"}, "_deposit": {"created_by": 18, "id": "50769", "owners": [18], "pid": {"revision_id": 0, "type": "depid", "value": "50769"}, "status": "published"}, "_oai": {"id": "oai:kanazawa-u.repo.nii.ac.jp:00050769", "sets": ["2829"]}, "author_link": ["88401", "88399"], "item_9_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2006-07-10", "bibliographicIssueDateType": "Issued"}, "bibliographicPageStart": "2p.", "bibliographicVolumeNumber": "2003-2004", "bibliographic_titles": [{"bibliographic_title": "平成16(2004)年度 科学研究費補助金 基盤研究(C) 研究成果報告書概要"}, {"bibliographic_title": "2004 Fiscal Year Final Research Report Summary", "bibliographic_titleLang": "en"}]}]}, "item_9_creator_33": {"attribute_name": "著者別表示", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "Honjo, Takaharu"}], "nameIdentifiers": [{"nameIdentifier": "88399", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "90019498", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=90019498"}]}]}, "item_9_description_21": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "環境試料として,幹線道路(国道8号線)沿道付近(中央分離帯)及びトンネル(国道8号線の倶利伽藍峠のトンネル,国道157号線の手取ダム近くの桑島隧道等)の車道周辺の土壌及び車道沿いに生育し表面にススを付着しているコケ植物等を採取した。採取試料は,電気乾燥機で80〜110℃で乾燥後,マイクロ波分解装置を用いて湿式分解を行い,フレームレス原子吸光法で定量した。\n結果は,国道8号線の地点(金沢市今町付近)では,コケ植物から,微量のPd(29〜59ng/g),Rh(15〜34ng/g)が検出されたが,Ptは\u003c8ng/g(検出限界)であった。一般に車道から1m内にPdとRhが検出された。このことは,貴金属粒子は比較的に重く,自動車の排気管から遠くへ移動せず,道路脇に落ちていることを示している。国道8号線の地点(北陸自動車道西インター付近)では,コケ植物(ギンゴケ)から1,270ng/gのPdが検出され,また土を含むギンゴケから2,950ng/gのPdが検出され,コケの表面を蒸留水で洗うとPdが検出限界以下となることから,Pdはコケの表面に他の固形のダストと共に付着していると思われる。国道8号線の倶利伽藍トンネル(石川県と富山県の県境)の出口と入り口では,自動車道の白線から1m内の土壌とコケ植物のPd, Rh及びPtは検出限界以下であった。この原因としては,自動車道の舗装が定期的に掃除されているためと思われる。国道157号線の地点(手取ダム付近の東二口隧道)では,トンネル内部の歩道の土(出入り口から150m,自動車白線から65〜95cm,車道からの高さ22cm)からは微量(57〜80ng/g)のPd及び歩道の隅にたまった泥から微量(290ng/g)のRhが検出され,トンネル内壁(地上から約1m)のススから微量(1,700ng/g)のRhが検出されたが,Ptは\u003c8ng/g(検出限界)であった。また,国道157号線の地点(手取ダム付近の桑島隧道)では,トンネル内部の歩道の土(出入り口から1〜130m,自動車白線から10〜90cm,車道からの高さ0〜22cm)からは微量(26〜84ng/g)のPd及び歩道の隅にたまった泥から微量(230ng/g)のRhが検出されたが,Ptは\u003c8ng/g(検出限界)であった。このように,環境中から微量のPdとRhが検出され,Ptは検出限界以下であったが,環境中での動態については不明な点も多く,今後の研究課題である。", "subitem_description_type": "Abstract"}, {"subitem_description": "Since automobiles equipped with three-way (i.e. removing carbon monoxide, nitrogen oxides, and hydrocarbons together in exhaust gasses) catalysts run under strict conditions as 400-1000 ℃, platinum, palladium, and rhodium are released by catalytic degradation, causing an environmental pollution. Then, the emissions of these precious metals in soot from the exhaust pipes and mufflers of 4 types of gasoline powered cars, were investigated first and ascertained that the values were Pt : 11-32 ppm, Pd : 7-19 ppm, and Rh : 3-25 ppm, respectively. The content of these precious metals tends to increase with increasing the running distance (50,000-130,000 km) of cars in roads, and also with drawing to the three-way catalytic converter in exhaust pipes.\nIn soot samples, Pd and Rh were detected in M IRA (DAIHATSU), while Pt and Rh were detected in FAMILIA (MAZDA), SUNNY (NISSAN), and SKYLINE (NISSAN), respectively. Inorganic ingredient (10.7-5,440 ppm) detected except for precious metals in soot of SKYLINE (running distance : 130,000km, 1992 type) were Na, Ca, Fe, Zn\u003eAl\u003eSi\u003eMg, Mn, Ni\u003eCe\u003eV, Zr, etc, while Ba, Co, La, and Mo were under detection limit.\nIn environmental samples involving soot of cars and dusts, as soil and moss (Bryum argenteum Hedw.) in major road ways (national road, the 8 line, Imamaehi, Kanazawa), Pd (29-59 ppb) and Rh (15-34 ppb) were detected within 1m from the edge of the white line of automobile road, while Pt were under detection limit (\u003c8ppb). This results indicate that these precious metalt particles emitted from motor vehicles are relatively heavy, and don\u0027t travel far from car exhaust pipes, falling out at the edges of roadways. In road ways of tunnel (national road, the 157 line, Higashifutaguchi and Kuwajima, near Tedori dam, Ishikawa), Pd (26-84 ppb) and Rh (230-1,700 ppb) were detected within 1 m from soil and soot of the inside wall, while Pt was under detection limit (8 ppb).\nSolubility of Pd and Rh in soot from the exhaust pipe and mufflers using 0.1 M hydrochloric acid were \u003c1%, while that of Pt was not observed. This result suggests that a small amount of Pd and Rh is in chloride species.", "subitem_description_type": "Abstract"}]}, "item_9_description_22": {"attribute_name": "内容記述", "attribute_value_mlt": [{"subitem_description": "研究課題/領域番号:15550064, 研究期間(年度):2003-2004", "subitem_description_type": "Other"}, {"subitem_description": "出典:研究課題「自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量」課題番号15550064\n(KAKEN:科学研究費助成事業データベース(国立情報学研究所)) \n(https://kaken.nii.ac.jp/report/KAKENHI-PROJECT-15550064/155500642004kenkyu_seika_hokoku_gaiyo/)を加工して作成", "subitem_description_type": "Other"}]}, "item_9_description_5": {"attribute_name": "提供者所属", "attribute_value_mlt": [{"subitem_description": "金沢大学自然科学研究科", "subitem_description_type": "Other"}]}, "item_9_identifier_registration": {"attribute_name": "ID登録", "attribute_value_mlt": [{"subitem_identifier_reg_text": "10.24517/00057077", "subitem_identifier_reg_type": "JaLC"}]}, "item_9_relation_28": {"attribute_name": "関連URI", "attribute_value_mlt": [{"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/search/?qm=90019498"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/search/?qm=90019498", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/grant/KAKENHI-PROJECT-15550064/"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/grant/KAKENHI-PROJECT-15550064/", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/report/KAKENHI-PROJECT-15550064/155500642004kenkyu_seika_hokoku_gaiyo/"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/report/KAKENHI-PROJECT-15550064/155500642004kenkyu_seika_hokoku_gaiyo/", "subitem_relation_type_select": "URI"}}]}, "item_9_version_type_25": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_ab4af688f83e57aa", "subitem_version_type": "AM"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "本浄, 高治"}], "nameIdentifiers": [{"nameIdentifier": "88401", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "90019498", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=90019498"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2022-05-19"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "TE-PR-HONJO-T-kaken 2006-2p.pdf", "filesize": [{"value": "87.4 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_11", "mimetype": "application/pdf", "size": 87400.0, "url": {"label": "TE-PR-HONJO-T-kaken 2006-2p.pdf", "url": "https://kanazawa-u.repo.nii.ac.jp/record/50769/files/TE-PR-HONJO-T-kaken 2006-2p.pdf"}, "version_id": "46034dda-b6a1-40ef-8615-9593fa2624f2"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "自動車排出ガス触媒", "subitem_subject_scheme": "Other"}, {"subitem_subject": "白金", "subitem_subject_scheme": "Other"}, {"subitem_subject": "パラジウム", "subitem_subject_scheme": "Other"}, {"subitem_subject": "ロジウム", "subitem_subject_scheme": "Other"}, {"subitem_subject": "環境", "subitem_subject_scheme": "Other"}, {"subitem_subject": "分離定量", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Determination", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Autocatalyst", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Platinum", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Palladium", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Rhodium", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Environment", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Separation", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Determination", "subitem_subject_language": "en", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "research report", "resourceuri": "http://purl.org/coar/resource_type/c_18ws"}]}, "item_title": "自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量"}, {"subitem_title": "Separation and Determination of Autocatalyst-Derived Platinum, Palladium, and Rhodium in the Environment", "subitem_title_language": "en"}]}, "item_type_id": "9", "owner": "18", "path": ["2829"], "permalink_uri": "https://doi.org/10.24517/00057077", "pubdate": {"attribute_name": "公開日", "attribute_value": "2022-05-19"}, "publish_date": "2022-05-19", "publish_status": "0", "recid": "50769", "relation": {}, "relation_version_is_last": true, "title": ["自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量"], "weko_shared_id": -1}
自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量
https://doi.org/10.24517/00057077
https://doi.org/10.24517/00057077d04cc208-2344-400b-a943-0ebce41d0ebd
名前 / ファイル | ライセンス | アクション |
---|---|---|
TE-PR-HONJO-T-kaken 2006-2p.pdf (87.4 kB)
|
Item type | 報告書 / Research Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2022-05-19 | |||||
タイトル | ||||||
タイトル | 自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | Separation and Determination of Autocatalyst-Derived Platinum, Palladium, and Rhodium in the Environment | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_18ws | |||||
資源タイプ | research report | |||||
ID登録 | ||||||
ID登録 | 10.24517/00057077 | |||||
ID登録タイプ | JaLC | |||||
著者 |
本浄, 高治
× 本浄, 高治 |
|||||
著者別表示 |
Honjo, Takaharu
× Honjo, Takaharu |
|||||
提供者所属 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 金沢大学自然科学研究科 | |||||
書誌情報 |
平成16(2004)年度 科学研究費補助金 基盤研究(C) 研究成果報告書概要 en : 2004 Fiscal Year Final Research Report Summary 巻 2003-2004, p. 2p., 発行日 2006-07-10 |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | 環境試料として,幹線道路(国道8号線)沿道付近(中央分離帯)及びトンネル(国道8号線の倶利伽藍峠のトンネル,国道157号線の手取ダム近くの桑島隧道等)の車道周辺の土壌及び車道沿いに生育し表面にススを付着しているコケ植物等を採取した。採取試料は,電気乾燥機で80〜110℃で乾燥後,マイクロ波分解装置を用いて湿式分解を行い,フレームレス原子吸光法で定量した。 結果は,国道8号線の地点(金沢市今町付近)では,コケ植物から,微量のPd(29〜59ng/g),Rh(15〜34ng/g)が検出されたが,Ptは<8ng/g(検出限界)であった。一般に車道から1m内にPdとRhが検出された。このことは,貴金属粒子は比較的に重く,自動車の排気管から遠くへ移動せず,道路脇に落ちていることを示している。国道8号線の地点(北陸自動車道西インター付近)では,コケ植物(ギンゴケ)から1,270ng/gのPdが検出され,また土を含むギンゴケから2,950ng/gのPdが検出され,コケの表面を蒸留水で洗うとPdが検出限界以下となることから,Pdはコケの表面に他の固形のダストと共に付着していると思われる。国道8号線の倶利伽藍トンネル(石川県と富山県の県境)の出口と入り口では,自動車道の白線から1m内の土壌とコケ植物のPd, Rh及びPtは検出限界以下であった。この原因としては,自動車道の舗装が定期的に掃除されているためと思われる。国道157号線の地点(手取ダム付近の東二口隧道)では,トンネル内部の歩道の土(出入り口から150m,自動車白線から65〜95cm,車道からの高さ22cm)からは微量(57〜80ng/g)のPd及び歩道の隅にたまった泥から微量(290ng/g)のRhが検出され,トンネル内壁(地上から約1m)のススから微量(1,700ng/g)のRhが検出されたが,Ptは<8ng/g(検出限界)であった。また,国道157号線の地点(手取ダム付近の桑島隧道)では,トンネル内部の歩道の土(出入り口から1〜130m,自動車白線から10〜90cm,車道からの高さ0〜22cm)からは微量(26〜84ng/g)のPd及び歩道の隅にたまった泥から微量(230ng/g)のRhが検出されたが,Ptは<8ng/g(検出限界)であった。このように,環境中から微量のPdとRhが検出され,Ptは検出限界以下であったが,環境中での動態については不明な点も多く,今後の研究課題である。 |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Since automobiles equipped with three-way (i.e. removing carbon monoxide, nitrogen oxides, and hydrocarbons together in exhaust gasses) catalysts run under strict conditions as 400-1000 ℃, platinum, palladium, and rhodium are released by catalytic degradation, causing an environmental pollution. Then, the emissions of these precious metals in soot from the exhaust pipes and mufflers of 4 types of gasoline powered cars, were investigated first and ascertained that the values were Pt : 11-32 ppm, Pd : 7-19 ppm, and Rh : 3-25 ppm, respectively. The content of these precious metals tends to increase with increasing the running distance (50,000-130,000 km) of cars in roads, and also with drawing to the three-way catalytic converter in exhaust pipes. In soot samples, Pd and Rh were detected in M IRA (DAIHATSU), while Pt and Rh were detected in FAMILIA (MAZDA), SUNNY (NISSAN), and SKYLINE (NISSAN), respectively. Inorganic ingredient (10.7-5,440 ppm) detected except for precious metals in soot of SKYLINE (running distance : 130,000km, 1992 type) were Na, Ca, Fe, Zn>Al>Si>Mg, Mn, Ni>Ce>V, Zr, etc, while Ba, Co, La, and Mo were under detection limit. In environmental samples involving soot of cars and dusts, as soil and moss (Bryum argenteum Hedw.) in major road ways (national road, the 8 line, Imamaehi, Kanazawa), Pd (29-59 ppb) and Rh (15-34 ppb) were detected within 1m from the edge of the white line of automobile road, while Pt were under detection limit (<8ppb). This results indicate that these precious metalt particles emitted from motor vehicles are relatively heavy, and don't travel far from car exhaust pipes, falling out at the edges of roadways. In road ways of tunnel (national road, the 157 line, Higashifutaguchi and Kuwajima, near Tedori dam, Ishikawa), Pd (26-84 ppb) and Rh (230-1,700 ppb) were detected within 1 m from soil and soot of the inside wall, while Pt was under detection limit (8 ppb). Solubility of Pd and Rh in soot from the exhaust pipe and mufflers using 0.1 M hydrochloric acid were <1%, while that of Pt was not observed. This result suggests that a small amount of Pd and Rh is in chloride species. |
|||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 研究課題/領域番号:15550064, 研究期間(年度):2003-2004 | |||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 出典:研究課題「自動車排出ガス触媒から遊離した環境中の白金,パラジウム及びロジウムの分離定量」課題番号15550064 (KAKEN:科学研究費助成事業データベース(国立情報学研究所)) (https://kaken.nii.ac.jp/report/KAKENHI-PROJECT-15550064/155500642004kenkyu_seika_hokoku_gaiyo/)を加工して作成 |
|||||
著者版フラグ | ||||||
出版タイプ | AM | |||||
出版タイプResource | http://purl.org/coar/version/c_ab4af688f83e57aa | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/search/?qm=90019498 | |||||
関連名称 | https://kaken.nii.ac.jp/search/?qm=90019498 | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/grant/KAKENHI-PROJECT-15550064/ | |||||
関連名称 | https://kaken.nii.ac.jp/grant/KAKENHI-PROJECT-15550064/ | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/report/KAKENHI-PROJECT-15550064/155500642004kenkyu_seika_hokoku_gaiyo/ | |||||
関連名称 | https://kaken.nii.ac.jp/report/KAKENHI-PROJECT-15550064/155500642004kenkyu_seika_hokoku_gaiyo/ |