{"_buckets": {"deposit": "45b9f8c5-4e49-4997-8e21-c186f3b5c113"}, "_deposit": {"created_by": 3, "id": "9735", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "9735"}, "status": "published"}, "_oai": {"id": "oai:kanazawa-u.repo.nii.ac.jp:00009735", "sets": ["936"]}, "author_link": ["14200", "485", "14199", "14201"], "item_4_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1997-07-15", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "7", "bibliographicPageEnd": "731", "bibliographicPageStart": "726", "bibliographicVolumeNumber": "46", "bibliographic_titles": [{"bibliographic_title": "材料=Journal of the Society of Materials Science, Japan"}]}]}, "item_4_description_21": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "The fatigue crack growth tests of WC-Co Cemented Carbides were carried out in a wide range of fatigue crack growth rate covering the threshold stress intensity factor range ΔK_\u003cth\u003e. The effects of the stress ratio, Co volume faction and the phase transformation of Co on the fatigue crack growth characteristics were investigated on the basis of fracture mechanics and fractography. The crack growth rate was measured using 3-point bending specimens. Crack growth tests were carried out at 10Hz and the stress ratio R=0.1 and 0.5. The main results obtained are as follows;(1)The Paris rule can be applied between da/dN and ΔK and it is shown to be da/dN=C(ΔK)^m.(2)The fractography of the fracture surface, shows that brittle fracture occurs in the Co binder phase at the stress rate R=0.1 but ductile fracture occurs in the Co binder phase at R=0.5. (3)The relation of da/dN-ΔK_\u003ceff\u003e/E of WC-Co cemented carbides shows the characteristic in the middle of the other metals and the alumina ceramics. (4)The Co binder phase undergoes phase transformation by repeated deformation and so it affects the characteristics delicately.", "subitem_description_type": "Abstract"}]}, "item_4_description_5": {"attribute_name": "提供者所属", "attribute_value_mlt": [{"subitem_description": "金沢大学大学院自然科学研究科", "subitem_description_type": "Other"}]}, "item_4_publisher_17": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本材料学会"}]}, "item_4_relation_28": {"attribute_name": "関連URI", "attribute_value_mlt": [{"subitem_relation_type_id": {"subitem_relation_type_id_text": "http://ci.nii.ac.jp/naid/110002293341/", "subitem_relation_type_select": "URI"}}]}, "item_4_rights_23": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "日本材料学会;本文データは日本材料学会の許諾に基づきCiNiiから複製したものである"}]}, "item_4_source_id_11": {"attribute_name": "NCID", "attribute_value_mlt": [{"subitem_source_identifier": "AN00096175", "subitem_source_identifier_type": "NCID"}]}, "item_4_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0514-5163", "subitem_source_identifier_type": "ISSN"}]}, "item_4_version_type_25": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "広瀬, 幸雄"}], "nameIdentifiers": [{"nameIdentifier": "485", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "20019425", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=20019425"}, {"nameIdentifier": "20019425", "nameIdentifierScheme": "研究者番号", "nameIdentifierURI": "https://nrid.nii.ac.jp/nrid/1000020019425"}]}, {"creatorNames": [{"creatorName": "夫, 明煥"}], "nameIdentifiers": [{"nameIdentifier": "14199", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "岸, 陽一"}], "nameIdentifiers": [{"nameIdentifier": "14200", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "朴, 栄哲"}], "nameIdentifiers": [{"nameIdentifier": "14201", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2017-10-03"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "TE-PR-HIROSE-Y-726.pdf", "filesize": [{"value": "958.1 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 958100.0, "url": {"label": "TE-PR-HIROSE-Y-726.pdf", "url": "https://kanazawa-u.repo.nii.ac.jp/record/9735/files/TE-PR-HIROSE-Y-726.pdf"}, "version_id": "1aca46bb-6848-4e4d-8b74-6a3b3ffb7172"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "Fatigue crack growth", "subitem_subject_scheme": "Other"}, {"subitem_subject": "WC-Co cemented carbides", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Stress intensity factor", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Stress ratio", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Phase transformation", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "WC-Co超硬合金の疲労き裂進展特性の評価(\u003c特集\u003eX線材料強度)", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "WC-Co超硬合金の疲労き裂進展特性の評価(\u003c特集\u003eX線材料強度)"}, {"subitem_title": "Evaluation of Fatigue Crack Growth Characteristics of WC-Co Cemented Carbides(Special Issue on X-Ray Study on Deformation and Fracture of Solid)", "subitem_title_language": "en"}]}, "item_type_id": "4", "owner": "3", "path": ["936"], "permalink_uri": "http://hdl.handle.net/2297/12322", "pubdate": {"attribute_name": "公開日", "attribute_value": "2017-10-03"}, "publish_date": "2017-10-03", "publish_status": "0", "recid": "9735", "relation": {}, "relation_version_is_last": true, "title": ["WC-Co超硬合金の疲労き裂進展特性の評価(\u003c特集\u003eX線材料強度)"], "weko_shared_id": -1}
WC-Co超硬合金の疲労き裂進展特性の評価(<特集>X線材料強度)
http://hdl.handle.net/2297/12322
http://hdl.handle.net/2297/12322d9e89fff-2ceb-4540-bf27-346d30b5baef
名前 / ファイル | ライセンス | アクション |
---|---|---|
TE-PR-HIROSE-Y-726.pdf (958.1 kB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2017-10-03 | |||||
タイトル | ||||||
タイトル | WC-Co超硬合金の疲労き裂進展特性の評価(<特集>X線材料強度) | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | Evaluation of Fatigue Crack Growth Characteristics of WC-Co Cemented Carbides(Special Issue on X-Ray Study on Deformation and Fracture of Solid) | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
著者 |
広瀬, 幸雄
× 広瀬, 幸雄× 夫, 明煥× 岸, 陽一× 朴, 栄哲 |
|||||
提供者所属 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 金沢大学大学院自然科学研究科 | |||||
書誌情報 |
材料=Journal of the Society of Materials Science, Japan 巻 46, 号 7, p. 726-731, 発行日 1997-07-15 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0514-5163 | |||||
NCID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN00096175 | |||||
出版者 | ||||||
出版者 | 日本材料学会 | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | The fatigue crack growth tests of WC-Co Cemented Carbides were carried out in a wide range of fatigue crack growth rate covering the threshold stress intensity factor range ΔK_<th>. The effects of the stress ratio, Co volume faction and the phase transformation of Co on the fatigue crack growth characteristics were investigated on the basis of fracture mechanics and fractography. The crack growth rate was measured using 3-point bending specimens. Crack growth tests were carried out at 10Hz and the stress ratio R=0.1 and 0.5. The main results obtained are as follows;(1)The Paris rule can be applied between da/dN and ΔK and it is shown to be da/dN=C(ΔK)^m.(2)The fractography of the fracture surface, shows that brittle fracture occurs in the Co binder phase at the stress rate R=0.1 but ductile fracture occurs in the Co binder phase at R=0.5. (3)The relation of da/dN-ΔK_<eff>/E of WC-Co cemented carbides shows the characteristic in the middle of the other metals and the alumina ceramics. (4)The Co binder phase undergoes phase transformation by repeated deformation and so it affects the characteristics delicately. | |||||
権利 | ||||||
権利情報 | 日本材料学会;本文データは日本材料学会の許諾に基づきCiNiiから複製したものである | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | http://ci.nii.ac.jp/naid/110002293341/ |