{"_buckets": {"deposit": "a1ca064e-f5a0-48d5-bad6-81736bfd7854"}, "_deposit": {"created_by": 18, "id": "53662", "owners": [18], "pid": {"revision_id": 0, "type": "depid", "value": "53662"}, "status": "published"}, "_oai": {"id": "oai:kanazawa-u.repo.nii.ac.jp:00053662", "sets": ["2818"]}, "author_link": ["80037", "80036"], "item_9_alternative_title_2": {"attribute_name": "その他のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "シンクロ型LPSO構造の材料科学: 次世代軽量構造材料への革新的展開"}, {"subitem_alternative_title": "Materials Science of synchronized LPSO structure: Innovative Development of Next-Generation Lightweight Structural Materials"}]}, "item_9_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2018-03-28", "bibliographicIssueDateType": "Issued"}, "bibliographicPageStart": "2p.", "bibliographicVolumeNumber": "2014-04-01 – 2016-03-31", "bibliographic_titles": [{"bibliographic_title": "平成27(2015)年度 科学研究費補助金 新学術領域研究(研究領域提案型) 研究実績の概要"}, {"bibliographic_title": "2015 Research Project Summary", "bibliographic_titleLang": "en"}]}]}, "item_9_creator_33": {"attribute_name": "著者別表示", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "Ishikawa, Kazuhiro"}], "nameIdentifiers": [{"nameIdentifier": "80037", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "10312448", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=10312448"}]}]}, "item_9_description_21": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "タイプⅡ型Mg-Gd-Zn合金の熱処理による組織および構造変化と水素化挙動について調べた。Mg85Zn6Gd9合金は鋳造状態でMgとZnGdからなる層状組織を形成していた。X線回折の結果、鋳造合金中に長周期性を有する相は観察されなかった。400℃でPCT試験を行ったところ、水素圧が0.1MPa以下で0.2H/M程度の水素を吸蔵することが分かった。さらに、1.3MPa付近で圧力プラトーが観察さた。vantHoff解析の結果、このプラトー圧の成因はMg+H2→MgH2反応に起因することが分かった。4MPaで1.8H/M程度の水素を吸蔵した。水素化後の試料中にはMgH2、GdH3、MgZn2が観察され、試料が完全に分解することが分かった。\nMg85Zn6Gd9合金をアルゴン雰囲気下で400℃で熱処理すると、鋳造状態で観察された層状組織は消失し、ZnGd母相中にMgリッチ相が析出した組織に変化した。X線回折の結果、2θ=4.8℃付近に長周期性を示すブラッグピークが観察された。熱処理によりMgリッチ相中にLPSO相が形成されたと考えられる。この合金を400℃でPCT測定すると、0.1MPaで0.2H/M程度の水素を吸蔵し、1.3MPa付近でプラトー圧が観察された。この合金の水素吸蔵特性は鋳造合金とほぼ同じであった。水素化後には、鋳造材と同様に試料は完全に分解しており、長周期性を有する相は観察できなかった。\n以上より、鋳造状態ではLPSO相が観察されない合金でも熱処理によりLPSO相が生成するが、LPSO相の安定性はそれほど高くないため、不均化反応により分解することが分かった。", "subitem_description_type": "Abstract"}]}, "item_9_description_22": {"attribute_name": "内容記述", "attribute_value_mlt": [{"subitem_description": "研究課題/領域番号:26109708, 研究期間(年度):2014-04-01 – 2016-03-31", "subitem_description_type": "Other"}, {"subitem_description": "出典:研究課題「水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明」課題番号26109708\n(KAKEN:科学研究費助成事業データベース(国立情報学研究所))\n(https://kaken.nii.ac.jp/ja/grant/KAKENHI-PUBLICLY-26109708/)を加工して作成", "subitem_description_type": "Other"}]}, "item_9_description_5": {"attribute_name": "提供者所属", "attribute_value_mlt": [{"subitem_description": "金沢大学理工研究域機械工学系", "subitem_description_type": "Other"}]}, "item_9_identifier_registration": {"attribute_name": "ID登録", "attribute_value_mlt": [{"subitem_identifier_reg_text": "10.24517/00059944", "subitem_identifier_reg_type": "JaLC"}]}, "item_9_relation_28": {"attribute_name": "関連URI", "attribute_value_mlt": [{"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/ja/search/?kw=10312448"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/ja/search/?kw=10312448", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/ja/grant/KAKENHI-PUBLICLY-26109708/"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/ja/grant/KAKENHI-PUBLICLY-26109708/", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/ja/grant/KAKENHI-AREA-2308/"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/ja/grant/KAKENHI-AREA-2308/", "subitem_relation_type_select": "URI"}}, {"subitem_relation_name": [{"subitem_relation_name_text": "https://kaken.nii.ac.jp/en/grant/KAKENHI-AREA-2308/"}], "subitem_relation_type_id": {"subitem_relation_type_id_text": "https://kaken.nii.ac.jp/en/grant/KAKENHI-AREA-2308/", "subitem_relation_type_select": "URI"}}]}, "item_9_version_type_25": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_ab4af688f83e57aa", "subitem_version_type": "AM"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "石川, 和宏"}], "nameIdentifiers": [{"nameIdentifier": "80036", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "10312448", "nameIdentifierScheme": "e-Rad", "nameIdentifierURI": "https://kaken.nii.ac.jp/ja/search/?qm=10312448"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2020-12-11"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "TE-PR-ISHIKAWA-K-kaken 2018-2p.pdf", "filesize": [{"value": "145.6 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_11", "mimetype": "application/pdf", "size": 145600.0, "url": {"label": "TE-PR-ISHIKAWA-K-kaken 2018-2p.pdf", "url": "https://kanazawa-u.repo.nii.ac.jp/record/53662/files/TE-PR-ISHIKAWA-K-kaken 2018-2p.pdf"}, "version_id": "632f287d-172f-419e-8a4d-6dd0ac4b11c5"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "LPSO", "subitem_subject_scheme": "Other"}, {"subitem_subject": "水素貯蔵", "subitem_subject_scheme": "Other"}, {"subitem_subject": "構造変化", "subitem_subject_scheme": "Other"}, {"subitem_subject": "X線回折", "subitem_subject_scheme": "Other"}, {"subitem_subject": "水素吸蔵", "subitem_subject_scheme": "Other"}, {"subitem_subject": "Mg合金", "subitem_subject_scheme": "Other"}, {"subitem_subject": "相安定性", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "research report", "resourceuri": "http://purl.org/coar/resource_type/c_18ws"}]}, "item_title": "水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明"}]}, "item_type_id": "9", "owner": "18", "path": ["2818"], "permalink_uri": "https://doi.org/10.24517/00059944", "pubdate": {"attribute_name": "公開日", "attribute_value": "2020-12-11"}, "publish_date": "2020-12-11", "publish_status": "0", "recid": "53662", "relation": {}, "relation_version_is_last": true, "title": ["水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明"], "weko_shared_id": -1}
水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明
https://doi.org/10.24517/00059944
https://doi.org/10.24517/0005994418803430-2966-4919-87ae-b4027f60e53a
名前 / ファイル | ライセンス | アクション |
---|---|---|
TE-PR-ISHIKAWA-K-kaken 2018-2p.pdf (145.6 kB)
|
Item type | 報告書 / Research Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2020-12-11 | |||||
タイトル | ||||||
タイトル | 水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_18ws | |||||
資源タイプ | research report | |||||
ID登録 | ||||||
ID登録 | 10.24517/00059944 | |||||
ID登録タイプ | JaLC | |||||
その他のタイトル | ||||||
その他のタイトル | シンクロ型LPSO構造の材料科学: 次世代軽量構造材料への革新的展開 | |||||
その他のタイトル | ||||||
その他のタイトル | Materials Science of synchronized LPSO structure: Innovative Development of Next-Generation Lightweight Structural Materials | |||||
著者別表示 |
Ishikawa, Kazuhiro
× Ishikawa, Kazuhiro |
|||||
提供者所属 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 金沢大学理工研究域機械工学系 | |||||
書誌情報 |
平成27(2015)年度 科学研究費補助金 新学術領域研究(研究領域提案型) 研究実績の概要 en : 2015 Research Project Summary 巻 2014-04-01 – 2016-03-31, p. 2p., 発行日 2018-03-28 |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | タイプⅡ型Mg-Gd-Zn合金の熱処理による組織および構造変化と水素化挙動について調べた。Mg85Zn6Gd9合金は鋳造状態でMgとZnGdからなる層状組織を形成していた。X線回折の結果、鋳造合金中に長周期性を有する相は観察されなかった。400℃でPCT試験を行ったところ、水素圧が0.1MPa以下で0.2H/M程度の水素を吸蔵することが分かった。さらに、1.3MPa付近で圧力プラトーが観察さた。vantHoff解析の結果、このプラトー圧の成因はMg+H2→MgH2反応に起因することが分かった。4MPaで1.8H/M程度の水素を吸蔵した。水素化後の試料中にはMgH2、GdH3、MgZn2が観察され、試料が完全に分解することが分かった。 Mg85Zn6Gd9合金をアルゴン雰囲気下で400℃で熱処理すると、鋳造状態で観察された層状組織は消失し、ZnGd母相中にMgリッチ相が析出した組織に変化した。X線回折の結果、2θ=4.8℃付近に長周期性を示すブラッグピークが観察された。熱処理によりMgリッチ相中にLPSO相が形成されたと考えられる。この合金を400℃でPCT測定すると、0.1MPaで0.2H/M程度の水素を吸蔵し、1.3MPa付近でプラトー圧が観察された。この合金の水素吸蔵特性は鋳造合金とほぼ同じであった。水素化後には、鋳造材と同様に試料は完全に分解しており、長周期性を有する相は観察できなかった。 以上より、鋳造状態ではLPSO相が観察されない合金でも熱処理によりLPSO相が生成するが、LPSO相の安定性はそれほど高くないため、不均化反応により分解することが分かった。 |
|||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 研究課題/領域番号:26109708, 研究期間(年度):2014-04-01 – 2016-03-31 | |||||
内容記述 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 出典:研究課題「水素化-脱水素化によるLPSO構造の安定性評価と形成過程の解明」課題番号26109708 (KAKEN:科学研究費助成事業データベース(国立情報学研究所)) (https://kaken.nii.ac.jp/ja/grant/KAKENHI-PUBLICLY-26109708/)を加工して作成 |
|||||
著者版フラグ | ||||||
出版タイプ | AM | |||||
出版タイプResource | http://purl.org/coar/version/c_ab4af688f83e57aa | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/ja/search/?kw=10312448 | |||||
関連名称 | https://kaken.nii.ac.jp/ja/search/?kw=10312448 | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/ja/grant/KAKENHI-PUBLICLY-26109708/ | |||||
関連名称 | https://kaken.nii.ac.jp/ja/grant/KAKENHI-PUBLICLY-26109708/ | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/ja/grant/KAKENHI-AREA-2308/ | |||||
関連名称 | https://kaken.nii.ac.jp/ja/grant/KAKENHI-AREA-2308/ | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://kaken.nii.ac.jp/en/grant/KAKENHI-AREA-2308/ | |||||
関連名称 | https://kaken.nii.ac.jp/en/grant/KAKENHI-AREA-2308/ |