{"_buckets": {"deposit": "bcd23fc7-904b-4b51-9feb-f18aeb22e856"}, "_deposit": {"created_by": 3, "id": "9366", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "9366"}, "status": "published"}, "_oai": {"id": "oai:kanazawa-u.repo.nii.ac.jp:00009366", "sets": ["936"]}, "author_link": ["13084", "12236", "13451", "13452"], "item_4_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "1998-01-01", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "9", "bibliographicPageEnd": "1329", "bibliographicPageStart": "1325", "bibliographicVolumeNumber": "64", "bibliographic_titles": [{"bibliographic_title": "精密工学会誌 = Journal of the Japan Society for Precision Engineering"}]}]}, "item_4_description_21": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Stainless steel pipe with fine hole and long size has recently been needed for the flow line of pure gas and liquid, which is used in the field of precision machinery. Inner wall polishing of the capillary is very difficult by ordinary finishing methods. High speed slurry flow finishing method developed by authors has been proved to have excellent polishing performance, but it has been needed a long time to obtain an acceptable level of surface roughness decrease. In the present study, effect of an annex of the glass beads into the slurry on the efficiency of finishing has been investigated. Experiments show that the medium of the glass beads annexed into the slurry has fine finishing characteristics rather than slurry medium. Surface roughness decreases with slurry flow pass number and its decreasing modes vary due to the property of medium. Optical micrographs of the medium indicate that the glass bead does not crush and not slenderize during finishing processes.", "subitem_description_type": "Abstract"}]}, "item_4_publisher_17": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "精密工学会 = The Japan Society for Precision Engineering"}]}, "item_4_relation_12": {"attribute_name": "DOI", "attribute_value_mlt": [{"subitem_relation_type": "isIdenticalTo", "subitem_relation_type_id": {"subitem_relation_type_id_text": "10.2493/jjspe.64.1325", "subitem_relation_type_select": "DOI"}}]}, "item_4_relation_28": {"attribute_name": "関連URI", "attribute_value_mlt": [{"subitem_relation_type_id": {"subitem_relation_type_id_text": "https://www.jstage.jst.go.jp/browse/jjspe/-char/ja/", "subitem_relation_type_select": "URI"}}, {"subitem_relation_type_id": {"subitem_relation_type_id_text": "http://www.jspe.or.jp/", "subitem_relation_type_select": "URI"}}]}, "item_4_rights_23": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "Copyright © The Japan Society for Precision Engineering 精密工学会"}]}, "item_4_source_id_11": {"attribute_name": "NCID", "attribute_value_mlt": [{"subitem_source_identifier": "AN1003250X", "subitem_source_identifier_type": "NCID"}]}, "item_4_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0912-0289", "subitem_source_identifier_type": "ISSN"}]}, "item_4_version_type_25": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "黒部, 利次"}], "nameIdentifiers": [{"nameIdentifier": "13084", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "60019742", "nameIdentifierScheme": "研究者番号", "nameIdentifierURI": "https://nrid.nii.ac.jp/nrid/1000060019742"}]}, {"creatorNames": [{"creatorName": "山田, 良穂"}], "nameIdentifiers": [{"nameIdentifier": "12236", "nameIdentifierScheme": "WEKO"}, {"nameIdentifier": "20126626", "nameIdentifierScheme": "研究者番号", "nameIdentifierURI": "https://nrid.nii.ac.jp/nrid/1000020126626"}]}, {"creatorNames": [{"creatorName": "山本, 桂一郎"}], "nameIdentifiers": [{"nameIdentifier": "13451", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "三浦, 毅彦"}], "nameIdentifiers": [{"nameIdentifier": "13452", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2017-10-03"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "TE-PR-KUROBE-T-1325.pdf", "filesize": [{"value": "6.3 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 6300000.0, "url": {"label": "TE-PR-KUROBE-T-1325.pdf", "url": "https://kanazawa-u.repo.nii.ac.jp/record/9366/files/TE-PR-KUROBE-T-1325.pdf"}, "version_id": "88e1bdb3-81ad-45b1-849d-bc98b94634e3"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "stainless steel capillary", "subitem_subject_scheme": "Other"}, {"subitem_subject": "inner wall polishing", "subitem_subject_scheme": "Other"}, {"subitem_subject": "surface roughness", "subitem_subject_scheme": "Other"}, {"subitem_subject": "glass beads", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "極細ステンレス鋼管内壁の高速流動研磨 (第3報): ガラスビーズ添加の効果", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "極細ステンレス鋼管内壁の高速流動研磨 (第3報): ガラスビーズ添加の効果"}, {"subitem_title": "High Speed Slurry Flow Finishing of Inner Wall of Stainless Steel Capillary (3rd Report): Effect of Annexed Glass Beads on Finishing Characteristics", "subitem_title_language": "en"}]}, "item_type_id": "4", "owner": "3", "path": ["936"], "permalink_uri": "http://hdl.handle.net/2297/42768", "pubdate": {"attribute_name": "公開日", "attribute_value": "2017-10-03"}, "publish_date": "2017-10-03", "publish_status": "0", "recid": "9366", "relation": {}, "relation_version_is_last": true, "title": ["極細ステンレス鋼管内壁の高速流動研磨 (第3報): ガラスビーズ添加の効果"], "weko_shared_id": -1}
極細ステンレス鋼管内壁の高速流動研磨 (第3報): ガラスビーズ添加の効果
http://hdl.handle.net/2297/42768
http://hdl.handle.net/2297/42768cceab1c1-c107-431e-b720-dabc68a16476
名前 / ファイル | ライセンス | アクション |
---|---|---|
TE-PR-KUROBE-T-1325.pdf (6.3 MB)
|
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2017-10-03 | |||||
タイトル | ||||||
タイトル | 極細ステンレス鋼管内壁の高速流動研磨 (第3報): ガラスビーズ添加の効果 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | High Speed Slurry Flow Finishing of Inner Wall of Stainless Steel Capillary (3rd Report): Effect of Annexed Glass Beads on Finishing Characteristics | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
著者 |
黒部, 利次
× 黒部, 利次× 山田, 良穂× 山本, 桂一郎× 三浦, 毅彦 |
|||||
書誌情報 |
精密工学会誌 = Journal of the Japan Society for Precision Engineering 巻 64, 号 9, p. 1325-1329, 発行日 1998-01-01 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0912-0289 | |||||
NCID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN1003250X | |||||
DOI | ||||||
関連タイプ | isIdenticalTo | |||||
識別子タイプ | DOI | |||||
関連識別子 | 10.2493/jjspe.64.1325 | |||||
出版者 | ||||||
出版者 | 精密工学会 = The Japan Society for Precision Engineering | |||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Stainless steel pipe with fine hole and long size has recently been needed for the flow line of pure gas and liquid, which is used in the field of precision machinery. Inner wall polishing of the capillary is very difficult by ordinary finishing methods. High speed slurry flow finishing method developed by authors has been proved to have excellent polishing performance, but it has been needed a long time to obtain an acceptable level of surface roughness decrease. In the present study, effect of an annex of the glass beads into the slurry on the efficiency of finishing has been investigated. Experiments show that the medium of the glass beads annexed into the slurry has fine finishing characteristics rather than slurry medium. Surface roughness decreases with slurry flow pass number and its decreasing modes vary due to the property of medium. Optical micrographs of the medium indicate that the glass bead does not crush and not slenderize during finishing processes. | |||||
権利 | ||||||
権利情報 | Copyright © The Japan Society for Precision Engineering 精密工学会 | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://www.jstage.jst.go.jp/browse/jjspe/-char/ja/ | |||||
関連URI | ||||||
識別子タイプ | URI | |||||
関連識別子 | http://www.jspe.or.jp/ |